Tuesday, 23 February 2021

The first stages of building the dinghy hull in the mould

First the two layers of Gelcoat on the mould

at so that it bonds with the gelcoat 


Then the second layer of CSM applied just as the first layer cured off. Then turn up the heating in the workshop for the rest of the day to keep the temperature up while the CSM and resin cures off then back tomorrow to apply the final two layers of CSM.





 